- Fe-Cr-Al Alloys
- Nickel-chromium Alloys
- Cn/Mn-Cu Alloys
- Cu-Ni Alloys
-
Precision Alloys
- Wire
- 1J330(1J30)
- 1J331(1J31)
- 1J332(1J32)
- 1J338(1J38)
- 1J350(1J50)
- 1J479(1J79)
- 1J485(1J85)
- 4J332(4J32)
- 4J332A(4J32A)
- 4J328(4j34)
- 4J329(4J29)
- 4J336(4J36)
- 4J342(4J42)
- 4J343(4J43)
- 4J352(4J49)
- 4J350(4J50)
- 6J415(6J15)
- 6J420(6J20)
- 6J422(6J22)
- 6J423(6J23)
- 6J424(6J24)
- 6J425(6J25)
- 6J426(6J26)
- 6J520(6J27)
- 6J525(6J28)
- Flat Wire
- 1J330(1J30)
- 1J331(1J31)
- 1J332(1J32)
- 1J338(1J38)
- 1J350(1J50)
- 1J479(1J79)
- 1J485(1J85)
- 4J332(4J32)
- 4J332A(4J32A)
- 4J328(4j34)
- 4J329(4J29)
- 4J336(4J36)
- 4J342(4J42)
- 4J343(4J43)
- 4J352(4J49)
- 4J350(4J50)
- 6J415(6J15)
- 6J420(6J20)
- 6J422(6J22)
- 6J423(6J23)
- 6J424(6J24)
- 6J425(6J25)
- 6J426(6J26)
- 6J520(6J27)
- 6J525(6J28)
- Flat Strip
- 1J330(1J30)
- 1J331(1J31)
- 1J332(1J32)
- 1J338(1J38)
- 1J350(1J50)
- 1J479(1J79)
- 1J485(1J85)
- 4J332(4J32)
- 4J332A(4J32A)
- 4J328(4j34)
- 4J329(4J29)
- 4J336(4J36)
- 4J342(4J42)
- 4J343(4J43)
- 4J352(4J49)
- 4J350(4J50)
- 6J415(6J15)
- 6J420(6J20)
- 6J422(6J22)
- 6J423(6J23)
- 6J424(6J24)
- 6J425(6J25)
- 6J426(6J26)
- 6J520(6J27)
- 6J525(6J28)
- Bar
- 1J330(1J30)
- 1J331(1J31)
- 1J332(1J32)
- 1J338(1J38)
- 1J350(1J50)
- 1J479(1J79)
- 1J485(1J85)
- 4J332(4J32)
- 4J332A(4J32A)
- 4J328(4j34)
- 4J329(4J29)
- 4J336(4J36)
- 4J342(4J42)
- 4J343(4J43)
- 4J352(4J49)
- 4J350(4J50)
- 6J415(6J15)
- 6J420(6J20)
- 6J422(6J22)
- 6J423(6J23)
- 6J424(6J24)
- 6J425(6J25)
- 6J426(6J26)
- 6J520(6J27)
- 6J525(6J28)
- Wire
- Ni-Al Alloys
- Pure Nickel Alloys
- Monel Alloys
- Hastelloy Alloys
- Inconel Alloys
- Incoloy Alloys
- Haynes Alloys
CuMn7SN Manganese Copper Alloy Flat Wire
Overview
CuMn7SN Manganese Copper Alloy Flat Wire is engineered for precision resistors and high-temperature applications, achieving an optimal balance of resistivity (0.34-0.38 μΩ·m) and tensile strength (550-700 MPa) through controlled manganese content (6.5-7.5% Mn). With superior oxidation and sulfidation resistance, it maintains stable performance from -50°C to 300°C, ideal for power electronics, industrial heaters, and automotive sensors. Compliant with IEC 60167 standards, offering fully traceable batch certifications.
Limiting Chemical Composition, %
Manganese(Mn)..............................................................................................................................6.5-7.5
Copper(Cu).....................................................................................................................................Balance
Tin(Sn)..............................................................................................................................................0.1-0.3
Iron(Fe)...............................................................................................................................................≤0.15
Other Impurities is Si, C, S strictly controlled,Total ≤0.3.
Technical Specifications
Parameter |
Value/Range |
Melting Point |
950-1020°C |
Tensile Strength |
550-700 MPa |
Elongation |
15-25% |
Surface Finish |
Bright Drawn/Nickel Plated |
Thickness Range |
1.0mm-5.0mm |
Width Range |
Customized (8mm-80mm) |
Temperature Resistance |
-50°C ~ 300°C |
Continuous Use Temp |
≤300°C |
Short-Term Peak Temp |
≤450°C (≤60 mins) |
Resistivity |
0.34-0.38 μΩ·m |
Density |
8.6±0.2 g/cm³ |
Material Properties
● Resistivity Stability:
TCR≤±50 ppm/°C ensures accuracy across temperatures
● Sulfidation Resistance:
Passes 3000hr ASTM B809 sulfur exposure test
● High Fatigue Life:
>10⁶ bending cycles (R=0.5mm radius)
● Solderability:
Compatible with Sn/Pb/Au coatings for reliable bonding
Core Advantages
● Precision Resistance Control:
±1% tolerance for medical-grade applications
● Environmental Durability:
Resists 85%RH humidity & salt spray (ASTM B117)
● Rapid Production Response:
72-hour expedited delivery available
Typical Applications
● Power Electronics:
High-current shunts, transformer windings
● Industrial Heating:
Injection molding heaters, hot runner system wiring
● Automotive Tech:
EV battery current sensors, oxygen sensor leads
● Test Equipment:
Standard resistors, bridge calibration components
Industries Served
● Renewable Energy & Energy Storage
● Industrial Automation & Robotics
● Automotive & EV Manufacturing
● Precision Instruments & Lab Equipment
● Power Transmission & Distribution
Packaging & Certifications
● Moisture/ESD-Proof: Vacuum-sealed spools with shock-absorbing liner, optional O₂-free packaging
● Certifications: IEC 60167, RoHS 2.0, ISO 9001:2015, ASTM F519
Why Choose CuMn7SN?
● Military-Grade Reliability:
Passes MIL-DTL-202H vibration & shock tests
● Global Logistics:
DDP incoterms & multi-port customs clearance
● Material Database:
Free access to temperature-resistance-stress profiles
Available Forms
We provide you with a variety of product forms, including but not limited to
● Strip & Foil
● Round Wire &Flat Wire
● Bar & Rod
● Electrothermal Strip
● Flange & Ring
● Wire & Welding
● Reststance Wire
● Electric Alloy Wire
● Electric Furnace Bar
● Customize
description2