- Fe-Cr-Al Alloys
- Nickel-chromium Alloys
- Cn/Mn-Cu Alloys
- Cu-Ni Alloys
-
Precision Alloys
- Wire
- 1J330(1J30)
- 1J331(1J31)
- 1J332(1J32)
- 1J338(1J38)
- 1J350(1J50)
- 1J479(1J79)
- 1J485(1J85)
- 4J332(4J32)
- 4J332A(4J32A)
- 4J328(4j34)
- 4J329(4J29)
- 4J336(4J36)
- 4J342(4J42)
- 4J343(4J43)
- 4J352(4J49)
- 4J350(4J50)
- 6J415(6J15)
- 6J420(6J20)
- 6J422(6J22)
- 6J423(6J23)
- 6J424(6J24)
- 6J425(6J25)
- 6J426(6J26)
- 6J520(6J27)
- 6J525(6J28)
- Flat Wire
- 1J330(1J30)
- 1J331(1J31)
- 1J332(1J32)
- 1J338(1J38)
- 1J350(1J50)
- 1J479(1J79)
- 1J485(1J85)
- 4J332(4J32)
- 4J332A(4J32A)
- 4J328(4j34)
- 4J329(4J29)
- 4J336(4J36)
- 4J342(4J42)
- 4J343(4J43)
- 4J352(4J49)
- 4J350(4J50)
- 6J415(6J15)
- 6J420(6J20)
- 6J422(6J22)
- 6J423(6J23)
- 6J424(6J24)
- 6J425(6J25)
- 6J426(6J26)
- 6J520(6J27)
- 6J525(6J28)
- Flat Strip
- 1J330(1J30)
- 1J331(1J31)
- 1J332(1J32)
- 1J338(1J38)
- 1J350(1J50)
- 1J479(1J79)
- 1J485(1J85)
- 4J332(4J32)
- 4J332A(4J32A)
- 4J328(4j34)
- 4J329(4J29)
- 4J336(4J36)
- 4J342(4J42)
- 4J343(4J43)
- 4J352(4J49)
- 4J350(4J50)
- 6J415(6J15)
- 6J420(6J20)
- 6J422(6J22)
- 6J423(6J23)
- 6J424(6J24)
- 6J425(6J25)
- 6J426(6J26)
- 6J520(6J27)
- 6J525(6J28)
- Bar
- 1J330(1J30)
- 1J331(1J31)
- 1J332(1J32)
- 1J338(1J38)
- 1J350(1J50)
- 1J479(1J79)
- 1J485(1J85)
- 4J332(4J32)
- 4J332A(4J32A)
- 4J328(4j34)
- 4J329(4J29)
- 4J336(4J36)
- 4J342(4J42)
- 4J343(4J43)
- 4J352(4J49)
- 4J350(4J50)
- 6J415(6J15)
- 6J420(6J20)
- 6J422(6J22)
- 6J423(6J23)
- 6J424(6J24)
- 6J425(6J25)
- 6J426(6J26)
- 6J520(6J27)
- 6J525(6J28)
- Wire
- Ni-Al Alloys
- Pure Nickel Alloys
- Monel Alloys
- Hastelloy Alloys
- Inconel Alloys
- Incoloy Alloys
- Haynes Alloys
Constantan Alloy Flat Strip 6j40
Overview
Constantan Alloy Flat Strip 6j40 is engineered for precision resistive applications with near-zero temperature coefficient (TCR≤±20ppm/°C), maintaining ±0.5% resistivity stability from -50°C to +400°C. Its superior oxidation resistance and fatigue performance make it ideal for industrial heaters, sensor bridges, and thermocouple compensation wires. ISO/IEC 17025 certified, 6J40 wire meets stringent material consistency requirements in medical and aerospace industries.
Limiting Chemical Composition, %
Nickel(Ni)............................................................................................................................................39.0-41.0
Manganese(Mn).....................................................................................................................................1.0-2.0
Copper(Cu)..................................................................................................................................................Rest
The Else is no
Technical Specifications
Parameter |
Value/Range |
Melting Point |
1210-1300°C |
Tensile Strength |
450-600 MPa |
Elongation |
20-30% |
Surface Finish |
Bright Annealed/Electropolished |
Thickness Range |
1.0mm-5.0mm |
Width Range |
Customized (8mm-80mm) |
Temperature Resistance |
-50°C ~ 400°C |
Continuous Use Temp |
≤400°C |
Short-Term Peak Temp |
≤550°C (≤30 mins) |
Resistivity |
0.49±0.02 μΩ·mm |
Density |
8.9±0.1 g/cm³ |
Material Properties
● Resistivity Stability:
ΔR/R≤0.5% across temperature range ensures measurement accuracy
● Low Thermal EMF:
Cu-Constantan pair EMF≤40μV/°C
● Creep Resistance:
<0.2% creep after 1000hrs at 400°C
● Surface Uniformity:
Ra≤0.1μm ultra-smooth surface minimizes contact resistance
Core Advantages
● Versatility:
Ideal for high-temperature, high-stress, and precision applications.
● Cost-Efficiency:
Extended lifespan reduces maintenance costs.
● Eco-Friendly Compliance:
Meets RoHS and ISO standards for sustainability.
Typical Applications
● Precision Measurement:
Strain gauge & Wheatstone bridge wiring
● Thermal Management:
Industrial furnace coils, semiconductor thermal control
● Energy Systems:
Fuel cell interconnects, solar thermal collectors
● Automotive Electronics:
Engine pressure sensors, BMS wiring
Industries Served
● Precision Instruments & Test Measurement
● Power Electronics & Energy Conversion
● Automotive & Rail Transport
● Medical Diagnostic Equipment
● Aerospace Thermal Management
Packaging & Certifications
● Anti-Oxidation Packaging: Inert gas-sealed spools + vacuum aluminum bags
● Certifications: ISO/IEC 17025, RoHS 3, REACH, UL 758
Why Choose 6J40?
● Zero-Compromise Quality:
Individual material analysis reports with ICP-OES testing
● Customization Service:
Resistivity fine-tuning (±5%) & specialty coating options
● Technical Support:
Free thermo-electro-mechanical simulation models
Available Forms
We provide you with a variety of product forms, including but not limited to
● Strip & Foil
● Round Wire &Flat Wire
● Bar & Rod
● Electrothermal Strip
● Flange & Ring
● Wire & Welding
● Reststance Wire
● Electric Alloy Wire
● Electric Furnace Bar
● Customize
description2