Leave Your Message
Featured Module
Products Categories
Electric Alloy Wire

Electric Alloy Wire

Electrothermal alloy wires make use of the resistance properties of the substance to create a heating element, and use the Joule effect to convert electrical energy into heat when an electric current passes through. It is usually made of metals or alloys with high resistivity and high thermal stability, such as nickel chromium alloy, iron chromium aluminum alloy, etc. These materials can generate a lot of heat when energized, and have good corrosion resistance and mechanical strength, ensuring that the heating wire can maintain stable performance under long-term use.


◆◆◆Availabe Pipes Materials◆◆◆

Fe-Cr-Al Alloy wire,  Fe-Cr-Al Alloy Flat Wire, Nickel-chromium alloy wire / Flat Wire, ect.

Specifications


◆ Dimensions:

Thickness: 0.1mm - 5mm

◆ Width: 0.5mm - 5mm ,Customized ,

Customized size needs to be confirmed with us

◆ Delivery State: Soft, ¼ hard, ½ hard, ¾ hard, hard

◆ Finish: 2B, BA, frosting, Mirror Finished, 8K, Hair Line with PVC, checkered plates, titanium


Standards

—Fe-Cr-Al Alloy wire
1Cr13Al4 0Cr15Al5 0Cr19Al2 0Cr21Al4 0Cr21Al6 0Cr25Al5 0Cr21Al6Nb 0Cr27Al7Mo2
—Fe-Cr-Al Alloy Flat Wire
1Cr13Al4 0Cr21Al4 0Cr21Al6 0Cr25Al5 0Cr21Al6Nb
—Nickel-chromium alloy wire / Flat Wire
Cr25Ni20 Cr20Ni30 Cr20Ni35 Cr15Ni60 Cr20Ni80 Cr30Ni70

Leave Your Message