Leave Your Message
Products Categories
Featured Module

Precision Alloys Flat Wire 4J336(4J36)

  • Place of Origin Jiangsu,China
  • Model Number Precision Alloys Flat Wire 4J336(4J36)
  • Trade Names FeNi36 flat wire,1.3918 flat wire
  • Dimensions Customized Size
  • Delivery Conditions Grinding. Polished. Bright.
  • Avaliable Shapes Wire.Customized
  • MOQ 50~200 (KG)
  • Production Standards GB/T、GJB、YB/T、ASTM、EN、DIN、IEC
  • Packaging Details Wooden Case, or as per Client's request
  • Payment Terms L/C, T/T, Western Union, MoneyGram
  • Trade Terms FOB, CIF, DDP, DAP, EXW
  • Delivery Time 20~60 days

Overview


Precision alloys have strict chemical composition control and fine microstructure, which can achieve high precision physical properties and meet the requirements of various precision equipment. Under different environmental conditions such as temperature, humidity and magnetic field, precision alloys can maintain stable physical properties to ensure long-term reliable operation of the equipment. Parts of various shapes and sizes can be made through various processing methods, such as forging, rolling, drawing, stamping, etc., to meet the needs of different application scenarios. Some precision alloys have good corrosion resistance and can be used in harsh environments to extend the service life of the equipment.



Precision alloy main properties


Alloy Nomenclature Chemical component(%)
Si  Mn Cr Ni Mo Co Cu Al Fe Other elements
1J330(1J30) 0.3 0.4   29.5-30.5         Rest  
1J331(1J31) 0.3 0.4   30.5-31.5         Rest  
1J332(1J32) 0.3 0.4   31.5-32.5       1-2 Rest  
1J336(1J36) 0.2 0.6   35-37         Rest  
1J338(1J38) 0.15-0.3 0.3-0.6 12.5-13.5 37.5-38.5         Rest  
1J348(1J48) 0.5 1   44-47 1.2-2.2   2.2-3.2   Rest  
1J350(1J50) 0.15-0.3 0.3-0.6   49-50.5     0.2   Rest  
1J479(1J79) 0.3-0.6 0.7-1.2   78-81.5 3.7-4.5       Rest  
1J485(1J85) 0.15-0.3 0.3-0.6   79-81 4.8-5.2   0.2   Rest  
4J332(4J32) 0.2 0.2-0.6   31.5-33   3.2-4.2 0.4-0.8   Rest  
4J332A(4J32A) 0.15-0.3 0.4   32-34.5   3.5-4.5     Rest Nb:0.2-0.3
4J328(4J34) 0.3 0.5   28.5-29.5   19.5-20.5     Rest  
4J329(4J29) 0.3 0.5 0.2 28.5-29.7 0.2 16.8-17.8 0.2   Rest The content of Al, Mg, Zr, Ti shall not be greater than 0.10 each, and the total content shall not be greater than 0.20.
4J336(4J36) 0.3 0.2-0.6   35-37         Rest  
4J342(4J42) 0.3 0.8   41-42.5   1   0.1 Rest  
4J343(4J43) 0.3 0.75-1.25   41-43         Rest  
4J352(4J49) 0.3 0.4 5-6 46-48         Rest B:0.03
4J350(4J50)
0.3 0.8   49.5-50.5       0.1 Rest  
6J415(6J15) 0.4-1.3 1.5 1.5-18 55-61       0.3 Rest  
6J420(6J20) 0.4-1.3 0.7 20-23 Rest       0.3 1.5  
6J422(6J22) 0.2 0.5-1.5 19-21.5 Rest       2.7-3.2 2-3  
6J423(6J23)
0.2 0.5-1.5 19-21.5 Rest     2-3 2.7-3.2    
6J424(6J24) 0.9-1.5 1-3 19-21.5 Rest       2-3.2 0.5  
6J425(6J25) 0.95-1.5 2.5-3 19-20 Rest       2.5-3 <0.5 Rare earth addition:0.1
6J426(6J26) 1-1.5 1-2 19.5-20.5 Rest       2.5-3.5 <0.5 Rare earth addition:0.1
6J520(6J27) 0.3 0.3 19.5-20.5         8.0-10.0 Rest Rare earth addition:0.1
6J525(6J28) 0.3 0.3 24.8-26.2         5.0-6.0 Rest V: 3.4-4.0
Rare earth addition:0.1



Standard product form


Wire flat wire strip bar machining products



Scope of application


Aerospace, electronics industry, automobile manufacturing, medical equipment, new energy, instrumentation



Available Forms


We provide you with a variety of product forms, including but not limited to


● Strip & Foil

● Round Wire &Flat Wire

● Bar & Rod

● Electrothermal Strip

● Flange & Ring

● Wire & Welding

● Reststance Wire

● Electric Alloy Wire

● Electric Furnace Bar

● Customize

description2

Leave Your Message