Leave Your Message
Products Categories
Featured Module

6J12 Manganese Copper Alloy Flat Strip

  • Place of Origin Jiangsu,China
  • Model Number 6J12 Manganese Copper Alloy Flat Strip
  • Trade Names MnCu6J12 flat strip, UNS C96400 flat strip, 2.1291 flat strip
  • Dimensions Customized Size
  • Delivery Conditions Grinding. Polished. Bright.
  • Avaliable Shapes Flat Strip.Customized
  • MOQ 50~200 (KG)
  • Production Standards GB/T、GJB、YB/T、ASTM、EN、DIN、IEC
  • Packaging Details Wooden Case, or as per Client's request
  • Payment Terms L/C, T/T, Western Union, MoneyGram
  • Trade Terms FOB, CIF, DDP, DAP, EXW
  • Delivery Time 20~60 days

Overview

6J12 Manganese Copper Alloy Flat Strip is a high-performance material engineered for applications requiring superior conductivity, heat resistance, and mechanical strength. Its optimized manganese-copper (Mn-Cu) ratio ensures stable resistivity and tensile performance, making it ideal for electronics, industrial heating systems, and precision instruments. With rigorous quality control, 6J12 wire maintains reliability under extreme temperatures, offering a premium alternative to conventional copper alloys.



Limiting Chemical Composition, %


Nickel(Ni)............................................................................................................................................2.0-3.0

Manganese(Mn).............................................................................................................................11.0-13.0

Copper(Cu)..............................................................................................................................................Rest

The Else is no



Main Properties


Performance / Nomenclature Constantan 6J40 Novokonstant 6J11 Manganin 6J12  F1 Manganin 6J8          F2 Manganin 6J13        
Main chemical composition Ni 39.0-41.0 — 2.0-3.0 — 2.0-5.0
Mn 1.0-2.0 10.5-12.5 11.0-13.0 8.0-10.0 11.0-13.0
Cu Rest Rest Rest Rest Rest
Else — Al:2.5-4.5
Fe:1.0-1.6
— Si:1.0-2.0 —
Service temperature
(℃)
5-500 5-500 5-450 10-480 10-480
Density
(g/cm³)
8.88 8 8.44 8.7 8.4
Resistivity at20℃
(200Cμ.m)
0.48±0.03 0.48±0.03 0.46±0.03 0.35±0.05 0.44±0.04
Temperature coefficient
x10-6/℃(20-600℃)
+40 +80 +20 +10 40
-40 -80 -3 -5
P-copper thermoelectric potential
(μV/℃)(0-100℃)
45 2 1 2 2
Elongation at rupture(%) ≥15 ≥15 ≥15 ≥15 ≥15



Technical Specifications


Parameter

Value/Range

Melting Point

950-1050°C

Tensile Strength

550-700 MPa

Elongation

18-25%

Surface Finish

Bright/Oxidation-Resistant

Thickness Range

1.0mm-5.0mm

Width Range

Customized (8mm-80mm)

Temperature Resistance

-50°C ~ 400°C

Continuous Use Temp

≤400°C

Short-Term Peak Temp

≤600°C (≤30 mins)

Resistivity

0.025-0.035 Ω·mm²/m

Density

8.5-8.9 g/cm³



Material Properties


● High Conductivity:

Low resistivity ensures efficient power transmission.


● Heat Resistance:

Continuous service temperature up to 400°C, short-term peak at 600°C.


● Mechanical Excellence:

High tensile strength and elongation for demanding fabrication.


● Corrosion Resistance:

Resists oxidation and chemical degradation.


Core Advantages


● Versatility:

Ideal for high-temperature, high-stress, and precision applications.


● Cost-Efficiency:

Extended lifespan reduces maintenance costs.


● Eco-Friendly Compliance:

Meets RoHS and ISO standards for sustainability.



Typical Applications


● Electronics:

Resistors, connectors, sensor components.


● Energy Systems:

Heating elements, fuses, power transmission parts.


● Automotive:

Engine harnesses, high-temperature sensors.


● Aerospace:

Heat-resistant cables and precision instruments.



Industries Served


● Electronics & Semiconductor Manufacturing

● Automotive & EV Industries

● Energy & Power Transmission

● Aerospace & Defense Technology

● Medical Devices & Precision Instruments



Packaging & Certifications


● Standard Packaging: Moisture-proof spools/plastic reels, customized wooden crates/pallets.

● Certifications: ISO 9001, RoHS, REACH compliant.



Why Choose 6J12?


● Performance Excellence:

Balances conductivity, strength, and heat resistance.


● Global Trust:

Trusted by 500+ clients worldwide.


● Technical Support:

Custom solutions and rapid after-sales service.



Available Forms


We provide you with a variety of product forms, including but not limited to


● Strip & Foil

● Round Wire &Flat Wire

● Bar & Rod

● Electrothermal Strip

● Flange & Ring

● Wire & Welding

● Reststance Wire

● Electric Alloy Wire

● Electric Furnace Bar

● Customize

description2

Leave Your Message