Inconel Alloys Wire Inconel 601
Overview
Inconel alloy 601 (UNSN06601/W.Nr. 2.4851) is a nickel-chromium alloy, that is highly resistant to oxidation through 2200°F. It is a general-purpose engineering material for applications that require resistance to heat and corrosion. An outstanding characteristic of INCONEL alloy 601 is its resistance to high temperature oxidation. Inconel 601 alloy develops a tightly adherent oxide scale which resists spalling even under severe thermal cycling.
The 601 alloy also has good resistance to aqueous corrosion, has high mechanical strength, and is readily formed, machined and welded.
What is more,the 601 alloy has good high temperature strength, and retains its ductility after long service exposure.
The properties of INCONEL alloy 601 make it a material of broad utility in such fields as thermal processing, chemical processing, pollution control,aerospace, and power generation.
Limiting Chemical Composition, %
Nickel (plus Cobalt)...............................................................................................................................................................58.00 min.
Chromium...........................................................................................................................................................................21.00-25 .00
Carbon......................................................................................................................................................................................0.10 max.
Manganese..............................................................................................................................................................................1.50 max.
Sulfur........................................................................................................................................................................................0.50 max.
Silicon......................................................................................................................................................................................0.015max.
Phosphorus..............................................................................................................................................................................0.02 max.
Aluminium.................................................................................................................................................................................1.70max.
Copper.......................................................................................................................................................................................1.00 max.
Main Properties
| Alloy Nomenclature → | Inconel 600 | Inconel 601 | Inconel 625 | Inconel X750 | Inconel 718 | |
| Performance ↓ | ||||||
| Main chemical composition | Ni | 72 | 60 | 61 | ≥70.0 | 50-55 |
| Cr | 15 | 23 | 21.5 | 14-17 | 17-21 | |
| Fe | 8 | 14 | ≤5.0 | ≤5.0 | Rest | |
| Mo | 0.5 | 1 | 9 | —— | 2.8-3.3 | |
| Al | 0.3 | 1.5 | ≤0.4 | 0.4-1.0 | 0.2-0.8 | |
| Ti | 0.3 | 0.5 | ≤0.4 | 2.25-2.75 | 0.65-1.15 | |
| Else | C≤0.15 | —— | Nb:3.6 C≤0.1 |
Nb:0.7-1.2 | Nb:4.75-5.5 | |
| Melting point(approx.)(℃) | 1370-1425℃ | 1350-1400℃ | 1290-1350℃ | 1393-1427℃ | 1260-1320℃ | |
| Density(g/cm³) | 8.47g/cm³ | 8.11g/cm³ | 8.44g/cm³ | 8.28g/cm³ | 8.24g/cm³ | |
Physical Constants
Density |
lb/in^3...........................................................................................0.293 |
g/cm^3............................................................................................8.11 | |
Specific Heat |
70°F,Btu/lb-°F. ..............................................................................0.107 |
21°C, J/kg-°C.................................................................................. 448 | |
Electrical Resistivity |
ohm-circ mil/ft................................................................................620 |
μΩ-m...............................................................................................1.03 | |
Curie Temperature |
°F..................................................................................................< -192 |
°C.................................................................................................< -196 | |
Melting Range |
°F..........................................................................................2480-2571 |
°C..........................................................................................1360-1411 | |
Permeability at 200 oersted (15.9 kA/m) |
76°F(24°C)....................................................................................1.003 |
-109°F (-78°C................................................................................1.004 | |
-320°F(-196°C )...........................................................................1.016 |
Mechanical properties
INCONEL alloy 601 has good mechanical strength.
The optimum condition for alloy 601 depends on the type of application and the service temperature involved. In general, the solution-treated condition is used for rupture-limited applications (temperatures of about 1000°F (540°C) and higher). The annealed condition is normally used for tensile-limited applications (temperatures below about 1000°F
(540°C)).
Yield Strength 0.2% offset |
Ultimate Tensile Strength |
Elongation |
||
psi |
Mpa |
psi |
Mpa |
% to 2" (51 mm) |
64000 |
440 |
115000 |
790 |
45 |
Tensile-properties
Short time elevated temperature tensile properties
The following table illustrates the short time tensile properties of Alloy 601 at temperatures
Test temperature |
Yield Strength 0.2% offset |
Ultimate Tensile Strength |
Elongation |
|||
°F |
°C |
psi |
Mpa |
psi |
Mpa |
% in 2" |
400 |
204 |
60000 |
415 |
109000 |
750 |
45 |
800 |
427 |
52000 |
360 |
102000 |
705 |
44 |
1000 |
538 |
48000 |
330 |
90000 |
620 |
44 |
1200 |
649 |
41000 |
280 |
60000 |
415 |
45 |
1400 |
760 |
26000 |
180 |
43000 |
235 |
70 |
1600 |
871 |
15000 |
105 |
18000 |
125 |
120 |
Corrosion Resistance
The high nickel and chromium composition of Alloy 601 not only help to give it superior high temperature performance but also bive the alloy excellent resistance to many wet corrosive environments. In these types of applications, the performance of Alloy 601 is similar to that of Alloy 600. Alloy 601 has excellent resistance to nitric acid, low concentrations of phosphoric acid, sodium hydroxide solutions and sea water. The alloy is not resistant to hydrochloric and hydrofluoric acid environments. Because of the alloys high nickel content, it is extremely resistant to chloride-ion stress-corrosion crackin in most environments
Available Forms
We provide you with a variety of product forms, including but not limited to
● Strip & Foil
● Round Wire &Flat Wire
● Bar & Rod
● Electrothermal Strip
● Flange & Ring
● Wire & Welding
● Reststance Wire
● Electric Alloy Wire
● Electric Furnace Bar
● Customize
description2

1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
6J12
6J8
6J13
6J40
CuMn7SN
CuMn30Ni5
6J12
6J8
6J13
6J40
CuMn7SN
CuMn30Ni5
6J12
6J8
6J13
6J40
CuMn7SN
CuMn30Ni5
6J12
6J8
6J13
6J40
CuMn7SN
CuMn30Ni5
CuNi30
CuNi34
CuNi44
CuNi30
CuNi34
CuNi44
CuNi30
CuNi34
CuNi44
CuNi30
CuNi34
CuNi44
4J336(4J36)
4J342(4J42)
4J343(4J43)
4J352(4J49)
4J350(4J50)
6J415(6J15)
6J420(6J20)
6J422(6J22)
6J423(6J23)
6J424(6J24)
6J425(6J25)
6J426(6J26)
6J520(6J27)
4J336(4J36)
4J342(4J42)
4J343(4J43)
4J352(4J49)
4J350(4J50)
6J415(6J15)
6J420(6J20)
6J422(6J22)
6J423(6J23)
6J424(6J24)
6J425(6J25)
6J426(6J26)
6J520(6J27)
4J336(4J36)
4J342(4J42)
4J343(4J43)
4J352(4J49)
4J350(4J50)
6J415(6J15)
6J420(6J20)
6J422(6J22)
6J423(6J23)
6J424(6J24)
6J425(6J25)
6J426(6J26)
6J520(6J27)
6J525(6J28)
4J336(4J36)
4J342(4J42)
4J343(4J43)
4J352(4J49)
4J350(4J50)
6J415(6J15)
6J420(6J20)
6J422(6J22)
6J423(6J23)
6J424(6J24)
6J425(6J25)
6J426(6J26)
6J520(6J27)
6J525(6J28)
Ni95Al5
monel 400
monel R405
monel K500
monel 502
monel 400
monel R405
monel K500
monel 502
monel R405
monel K500
monel 502
Hastelloy C-22
Hastelloy C-22
Hastelloy C-22
Inconel 800
Inconel 800H
Inconel 800HT
Inconel 825
Inconel 800
Inconel 800H
Inconel 800HT
Inconel 825
Inconel 800
Inconel 800H
Inconel 800HT
Inconel 825
Strip & Foil
Round Wire
Bar & Rod
Electrothermal strip
Bolts & Fasteners
Flange & Ring
Wire & Welding
Reststance wire & flat wire
Electric alloy wire
Electric furnace wire