Leave Your Message
Products Categories
Featured Module

Nickel-chromium Alloys Bar Cr20Ni80

  • Place of Origin Jiangsu,China
  • Model Number Nickel-chromium Alloys Bar Cr20Ni80
  • Trade Names NiCr80/20 bar,Cr20Ni80 Bar,UNS N06003 bar,2.4869 bar
  • Dimensions Customized Size
  • Delivery Conditions Grinding. Polished. Bright.
  • Avaliable Shapes Wire.Customized
  • MOQ 50~200 (KG)
  • Production Standards GB/T、GJB、YB/T、ASTM、EN、DIN、IEC
  • Packaging Details Wooden Case, or as per Client's request
  • Payment Terms L/C, T/T, Western Union, MoneyGram
  • Trade Terms FOB, CIF, DDP, DAP, EXW
  • Delivery Time 20~60 days

Overview

Cr20Ni80 Nickel-Chromium Alloy Bar is a high-nickel (80%) resistance alloy designed for high-efficiency heating elements, offering exceptional resistivity, oxidation resistance, and long-term thermal stability. Capable of continuous operation up to 1200°C with a protective oxide layer, it is widely used in industrial electric furnaces, household heaters, high-temperature sensors, and new energy equipment, making it the top choice for energy efficiency and reliability.



Limiting Chemical Composition, %


Chromium(Cr)..................................................................................................................................15.0

Aluminum(Ni)..................................................................................................................................60.0

Balance Iron (Fe) & Trace Elements



Main Properties


Alloy Nomenclature → Cr20Ni80 Cr30Ni70 Cr15Ni60 Cr20Ni35 Cr20Ni30 Cr25Ni20
Performance ↓
Main chemical composition Ni Rest Rest 55-61 34-37 30-34 19-22
Cr 20-23 28-31 15-18 18-21 18-21 23-27
Fe ≤1.0 ≤1.0 Rest Rest Rest Rest
Max.Continuous service
temp.of element(℃)
1200 1250 1150 1100 1100 950
(Ω·mm²/m)
Resistivity at20℃
1.09 1.18 1.12 1.04 1.04 0.96
Density(g/cm³) 8.4 8.1 8.2 7.9 7.9 8



Material Characteristics


Density

about 8.5g/cm³

Resistivity

1.10 μΩ·m (20°C)

Temperature Range

Continuous Service 1150°C, Short-Term Peak 1250°C



Material Properties


●Ultra-High Resistivity:

1.10 μΩ·m (20°C) for efficient electrical-to-heat conversion.


● Extreme Oxidation Resistance:

Oxidation rate <0.5 g/m²·h at 1200°C for extended service life.


● Broad Temperature Stability:

Minimal mechanical degradation from -50°C to 1200°C.



Core Advantages


● Energy Savings:

Stable resistivity ensures uniform heating, reducing energy consumption by 15%-25%.


● Maintenance-Free:

Oxidation and carburization resistance minimize downtime.


● Flexible Processing:

Compatible with ultra-fine wire drawing (≥0.03mm) and complex coiling.



Typical Applications


● Industrial Heating Systems:

Resistance wires, furnace heating elements, heat treatment fixtures.

● Consumer Electronics:

Hair dryer coils, coffee machine tubes, instant water heaters.

● New Energy:

Fuel cell heaters, lithium battery sintering furnace components.



Technical Parameters


ParameterNumericUnit
Melting Point1400-1450℃
Tensile Strength≥620MPa
Elongation≥20%
Surface FinishBright / Annealed-
Thickness Range0.1-30.0 (Supports ultra-thin customization)mm
Width Range1-150(Support narrow band/silk)mm



Applicable Industries


● Home Appliances & Consumer Electronics

● Industrial Thermal Processing

● New Energy & Energy Storage

● Automotive Heating Systems

● Scientific Research Equipment



Packaging & Certifications


● Packaging:

Anti-static spools + vacuum sealing (for wires); anti-rust crates + desiccants (for bars).


● Certifications:

Compliant with ASTM B344, IEC 60216, RoHS; material composition analysis reports available.



Why Choose This Product?


● Industry-Leading Performance:

80% nickel content ensures top-tier resistivity stability and high-temperature longevity.


● Full Customization:

Wire, strip, and custom-shaped parts processing available.


● Traceable Quality:

Full chemical and mechanical test reports for each batch.



Available Forms


We provide you with a variety of product forms, including but not limited to


● Strip & Foil

● Round Wire &Flat Wire

● Bar & Rod

● Electrothermal Strip

● Flange & Ring

● Wire & Welding

● Reststance Wire

● Electric Alloy Wire

● Electric Furnace Bar

● Customize

description2

Leave Your Message