Inconel Alloys Wire & Welding Inconel 601

  • Place of Origin Jiangsu,China
  • Model Number Inconel Alloys Wire & Welding Inconel 601
  • Trade Names UNSN06601/W.Nr. 2.4851
  • Dimensions Customized Size
  • Delivery Conditions Grinding. Polished. Bright.
  • Avaliable Shapes Wire, Flat Wire, Flat Strip, Steel Bar, Bolts, Fasteners, Flange & Ring, Wire & Welding, Customized
  • MOQ 50~200 (KG)
  • Production Standards ASTM B167,B829,B775,B516,B751,B366,B166,B168,B906,AWS A5.14 ERNiCrFe-11
  • Packaging Details Wooden Case, or as per Client's request
  • Payment Terms L/C, T/T, Western Union, MoneyGram
  • Trade Terms FOB, CIF, DDP, DAP, EXW
  • Delivery Time 20~60 days

Overview


Inconel alloy 601 (UNSN06601/W.Nr. 2.4851) is a nickel-chromium alloy, that is highly resistant to oxidation through 2200°F. It is a general-purpose engineering material for applications that require resistance to heat and corrosion. An outstanding characteristic of INCONEL alloy 601 is its resistance to high temperature oxidation. Inconel 601 alloy develops a tightly adherent oxide scale which resists spalling even under severe thermal cycling.

The 601 alloy also has good resistance to aqueous corrosion, has high mechanical strength, and is readily formed, machined and welded.

What is more,the 601 alloy has good high temperature strength, and retains its ductility after long service exposure.

The properties of INCONEL alloy 601 make it a material of broad utility in such fields as thermal processing, chemical processing, pollution control,aerospace, and power generation.


Limiting Chemical Composition, %


Nickel (plus Cobalt)...............................................................................................................................................................58.00 min.

Chromium...........................................................................................................................................................................21.00-25 .00

Carbon......................................................................................................................................................................................0.10 max.

Manganese..............................................................................................................................................................................1.50 max.

Sulfur........................................................................................................................................................................................0.50 max.

Silicon......................................................................................................................................................................................0.015max.

Phosphorus..............................................................................................................................................................................0.02 max.

Aluminium.................................................................................................................................................................................1.70max.

Copper.......................................................................................................................................................................................1.00 max.



Main Properties


Alloy Nomenclature → Inconel 600 Inconel 601 Inconel 625 Inconel X750 Inconel 718
Performance ↓
Main chemical composition Ni 72 60 61 ≥70.0 50-55
Cr 15 23 21.5 14-17 17-21
Fe 8 14 ≤5.0 ≤5.0 Rest
Mo 0.5 1 9 —— 2.8-3.3
Al 0.3 1.5 ≤0.4 0.4-1.0 0.2-0.8
 Ti 0.3 0.5 ≤0.4 2.25-2.75 0.65-1.15
Else C≤0.15 —— Nb:3.6
C≤0.1
Nb:0.7-1.2 Nb:4.75-5.5
Melting point(approx.)(℃) 1370-1425℃ 1350-1400℃ 1290-1350℃ 1393-1427℃ 1260-1320℃
Density(g/cm³) 8.47g/cm³ 8.11g/cm³ 8.44g/cm³ 8.28g/cm³ 8.24g/cm³



Physical Constants


Density

lb/in^3...........................................................................................0.293

g/cm^3............................................................................................8.11

Specific Heat

70°F,Btu/lb-°F. ..............................................................................0.107

21°C, J/kg-°C.................................................................................. 448

Electrical Resistivity

ohm-circ mil/ft................................................................................620

μΩ-m...............................................................................................1.03

Curie Temperature

°F..................................................................................................< -192

°C.................................................................................................< -196

Melting Range

°F..........................................................................................2480-2571

°C..........................................................................................1360-1411

Permeability at 200 oersted (15.9 kA/m)

76°F(24°C)....................................................................................1.003

-109°F (-78°C................................................................................1.004

-320°F(-196°C )...........................................................................1.016



Mechanical properties


INCONEL alloy 601 has good mechanical strength.

The optimum condition for alloy 601 depends on the type of application and the service temperature involved. In general, the solution-treated condition is used for rupture-limited applications (temperatures of about 1000°F (540°C) and higher). The annealed condition is normally used for tensile-limited applications (temperatures below about 1000°F

(540°C)).


Yield Strength 0.2% offset

Ultimate Tensile Strength

Elongation

psi

Mpa

psi

Mpa

% to 2" (51 mm)

64000

440

115000

790

45



Tensile-properties


Short time elevated temperature tensile properties

The following table illustrates the short time tensile properties of Alloy 601 at temperatures


Test temperature

Yield Strength 0.2% offset

Ultimate Tensile Strength

Elongation

°F

°C

psi

Mpa

psi

Mpa

% in 2"

400

204

60000

415

109000

750

45

800

427

52000

360

102000

705

44

1000

538

48000

330

90000

620

44

1200

649

41000

280

60000

415

45

1400

760

26000

180

43000

235

70

1600

871

15000

105

18000

125

120



Corrosion Resistance


The high nickel and chromium composition of Alloy 601 not only help to give it superior high temperature performance but also bive the alloy excellent resistance to many wet corrosive environments. In these types of applications, the performance of Alloy 601 is similar to that of Alloy 600. Alloy 601 has excellent resistance to nitric acid, low concentrations of phosphoric acid, sodium hydroxide solutions and sea water. The alloy is not resistant to hydrochloric and hydrofluoric acid environments. Because of the alloys high nickel content, it is extremely resistant to chloride-ion stress-corrosion crackin in most environments



Available Forms


We provide you with a variety of product forms, including but not limited to


● Strip & Foil

● Round Wire &Flat Wire

● Bar & Rod

● Electrothermal Strip

● Flange & Ring

● Wire & Welding

● Reststance Wire

● Electric Alloy Wire

● Electric Furnace Bar

● Customize

description2

Leave Your Message