Nickel-chromium Alloys Wire Cr25Ni20

  • Place of Origin Jiangsu,China
  • Model Number Nickel-chromium Alloys Wire Cr25Ni20
  • Trade Names Cr25Ni20,Ni20Cr25
  • Dimensions Customized Size
  • Delivery Conditions Grinding. Polished. Bright.
  • Avaliable Shapes Wire.Customized
  • MOQ 50~200 (KG)
  • Production Standards GB/T、GJB、YB/T、ASTM、EN、DIN、IEC
  • Packaging Details Wooden Case, or as per Client's request
  • Payment Terms L/C, T/T, Western Union, MoneyGram
  • Trade Terms FOB, CIF, DDP, DAP, EXW
  • Delivery Time 20~60 days

Overview

Cr25Ni20 nickel chromium alloy round wire is a high-performance material designed for high-temperature applications. With excellent oxidation resistance and thermal stability, it is widely used in electric heating elements, industrial furnaces, and resistance heating systems. Its durability ensures reliable performance in extreme environments.



Limiting Chemical Composition, %


Chromium(Cr)..................................................................................................................................25.0

Nickel(Ni).........................................................................................................................................20.0

Balance Iron (Fe) & Trace Elements



Main Properties


Alloy Nomenclature → Cr20Ni80 Cr30Ni70 Cr15Ni60 Cr20Ni35 Cr20Ni30 Cr25Ni20
Performance ↓
Main chemical composition Ni Rest Rest 55-61 34-37 30-34 19-22
Cr 20-23 28-31 15-18 18-21 18-21 23-27
Fe ≤1.0 ≤1.0 Rest Rest Rest Rest
Max.Continuous service
temp.of element(℃)
1200 1250 1150 1100 1100 950
(Ω·mm²/m)
Resistivity at20℃
1.09 1.18 1.12 1.04 1.04 0.96
Density(g/cm³) 8.4 8.1 8.2 7.9 7.9 8



Material Characteristics


Density

about 7.9g/cm³

Resistivity

1.12 μΩ·m (20℃)

Temperature Range

Continuous Service 1000℃~1200℃, Short-Term Peak 1250℃



Key Advantages


● Superior Oxidation Resistance:

High chromium content (25% Cr) forms a dense Cr₂O₃ oxide layer, significantly reducing high-temperature oxidation rate.


● Long Service Life:

Stable mechanical strength and excellent creep resistance under high temperatures, extending component replacement intervals.


● Broad Compatibility:

Suitable for both oxidizing and neutral atmospheres, ideal for industrial furnaces and heat treatment systems.


Typical Applications


● Industrial Heating Elements:

Resistance wires and heating elements for metallurgical annealing furnaces, ceramic sintering kilns, and glass melting furnaces.


● Heat Treatment Equipment:

Radiant tubes for continuous heat treatment furnaces, muffle furnace linings.


● High-Temperature Sensors:

Thermocouple protection sheaths, conductive components in extreme heat.



Material Characteristics


ParameterNumericUnit
Melting Point1400-1420℃
Tensile Strength≥650MPa
Elongation≥20%
Surface FinishBright/Oxidized-
Diameter Range0.1-6.0mm



Target Industries


● Metallurgy

● Ceramics & Glass Manufacturing

● Chemical Processing

● Heat Treatment & Foundry



Packaging & Certifications


● Packaging:

Moisture-proof spools/wooden cases, custom lengths (≤500m/coil).


● Certifications:

ASTM B344, IEC 60216, RoHS Compliance.



Why Choose Cr25Ni20?


● Cost-Effective:

Outstanding price-performance ratio among high-temperature alloys, ideal for large-scale industrial heating.


● Customization:

Available in non-standard diameters, surface finishes, and specialized annealing processes.



Available Forms


We provide you with a variety of product forms, including but not limited to


● Strip & Foil

● Round Wire &Flat Wire

● Bar & Rod

● Electrothermal Strip

● Flange & Ring

● Wire & Welding

● Reststance Wire

● Electric Alloy Wire

● Electric Furnace Bar

● Customize

description2

Leave Your Message