Nickel-chromium Alloys Flat Wire Cr25Ni20

  • Place of Origin Jiangsu,China
  • Model Number Nickel-chromium Alloys Flat Wire Cr25Ni20
  • Trade Names UNS N06010 flat wire
  • Dimensions Customized Size
  • Delivery Conditions Grinding. Polished. Bright.
  • Avaliable Shapes Wire.Customized
  • MOQ 50~200 (KG)
  • Production Standards GB/T、GJB、YB/T、ASTM、EN、DIN、IEC
  • Packaging Details Wooden Case, or as per Client's request
  • Payment Terms L/C, T/T, Western Union, MoneyGram
  • Trade Terms FOB, CIF, DDP, DAP, EXW
  • Delivery Time 20~60 days

Overview

Cr25Ni20 Nickel-Chromium Alloy Flat Wire is a high-performance material designed for extreme temperature environments, offering exceptional oxidation resistance, high tensile strength, and superior elongation. Widely used in heating elements, industrial furnaces, household appliances, and aerospace industries. Custom sizes available for diverse applications.



Limiting Chemical Composition, %


Chromium..................................................................................................................................25.0

Aluminum..................................................................................................................................20.0

Fe & trace elements



Main Properties


Alloy Nomenclature → Cr20Ni80 Cr30Ni70 Cr15Ni60 Cr20Ni35 Cr20Ni30 Cr25Ni20
Performance ↓
Main chemical composition Ni Rest Rest 55-61 34-37 30-34 19-22
Cr 20-23 28-31 15-18 18-21 18-21 23-27
Fe ≤1.0 ≤1.0 Rest Rest Rest Rest
Max.Continuous service
temp.of element(℃)
1200 1250 1150 1100 1100 950
(Ω·mm²/m)
Resistivity at20℃
1.09 1.18 1.12 1.04 1.04 0.96
Density(g/cm³) 8.4 8.1 8.2 7.9 7.9 8



Material Characteristics


Density

about 8.4g/cm³

Resistivity

1.08 μΩ·m (20°C)

Temperature Range

Continuous Service ≤1200℃, Short-Term Peak ≤1400℃



Material Properties


● High-Temperature Resistance:

Stable operation up to 1200°C.


● Oxidation Resistance:

Forms a protective oxide layer at high temperatures.


● High Electrical Efficiency:

Low resistivity ensures efficient energy conversion.



Core Advantages


● Long Service Life:

Superior creep and fatigue resistance.


● Customizable:

Available in thickness 0.1-5mm, width 1-50mm.


● Eco-Friendly:

Compliant with RoHS standards.



Typical Applications


● Heating Elements:

Industrial furnace wires, heating tubes.


● Aerospace:

Engine components, high-temperature sensors.


● Household Appliances:

Electric kettles, iron heating plates.



Technical Specifications


ParameterNumericUnit
Melting Point1400-1420℃
Tensile Strength≥650MPa
Elongation≥35%
Surface FinishBright/Oxidized-
Thickness0.1-5.0mm
Width1-50mm



Target Industries


● Electric Heating Equipment

● Industrial Furnaces & Heat Treatment

● Household Appliances & Electronics

● Aerospace & Automotive



Packaging & Certifications


● Standard Packaging:

Moisture-proof wooden crates or pallets.


● Certifications:

ISO 9001, RoHS, SGS Test Reports.



Why Choose Us?


● Quality Assurance:

Rigorous inspection for consistent performance.


● Fast Delivery:

7-15 days for small-batch orders.


● Global Service:

Exported to 50+ countries.



Available Forms


We provide you with a variety of product forms, including but not limited to


● Strip & Foil

● Round Wire &Flat Wire

● Bar & Rod

● Electrothermal Strip

● Flange & Ring

● Wire & Welding

● Reststance Wire

● Electric Alloy Wire

● Electric Furnace Bar

● Customize

description2

Leave Your Message