Nickel-chromium Alloys Flat Wire Cr30Ni70

  • Place of Origin Jiangsu,China
  • Model Number Nickel-chromium Alloys Flat Wire Cr30Ni70
  • Trade Names Ultra-High Temp Industrial Material
  • Dimensions Customized Size
  • Delivery Conditions Grinding. Polished. Bright.
  • Avaliable Shapes Wire.Customized
  • MOQ 50~200 (KG)
  • Production Standards GB/T、GJB、YB/T、ASTM、EN、DIN、IEC
  • Packaging Details Wooden Case, or as per Client's request
  • Payment Terms L/C, T/T, Western Union, MoneyGram
  • Trade Terms FOB, CIF, DDP, DAP, EXW
  • Delivery Time 20~60 days

Overview

Cr30Ni70 Nickel-Chromium Alloy Flat Wire delivers exceptional corrosion resistance and ultra-high temperature stability (up to 1250°C) with a high nickel content (70% Ni), tensile strength ≥780 MPa, and low resistivity (1.05 μΩ·m at 20°C). Featuring customizable surface finishes (bright annealed/pickled) and precision dimensions (thickness 0.1-12mm, width 5-200mm), it is engineered for chemical processing, industrial furnaces, aerospace, and new energy applications under extreme conditions.



Limiting Chemical Composition, %


Chromium..................................................................................................................................30.0

Aluminum..................................................................................................................................70.0

Fe & trace elements



Main Properties


Alloy Nomenclature → Cr20Ni80 Cr30Ni70 Cr15Ni60 Cr20Ni35 Cr20Ni30 Cr25Ni20
Performance ↓
Main chemical composition Ni Rest Rest 55-61 34-37 30-34 19-22
Cr 20-23 28-31 15-18 18-21 18-21 23-27
Fe ≤1.0 ≤1.0 Rest Rest Rest Rest
Max.Continuous service
temp.of element(℃)
1200 1250 1150 1100 1100 950
(Ω·mm²/m)
Resistivity at20℃
1.09 1.18 1.12 1.04 1.04 0.96
Density(g/cm³) 8.4 8.1 8.2 7.9 7.9 8



Material Characteristics


Density

about 8.3g/cm³

Resistivity

1.05 μΩ·m (20°C)

Temperature Range

Continuous Service 1100°C~1250°C, Short-Term Peak ≤1400℃



Material Properties


● Ultra-High Temp & Creep Resistance:

Stable operation at 1100~1250°C with superior creep resistance.


● High-Nickel Corrosion Resistance:

Resists acids, alkalis, and salt spray corrosion.


● Low Resistivity & High Efficiency:

1.05 μΩ·m (20°C) for energy-saving performance.


● Custom Surface Finish:

Bright annealed, pickled, brushed, or polished.



Core Advantages


● Broad Sizing Range:

Thickness 0.1-12mm, width 5-200mm (±0.01mm tolerance).


● Self-Healing Oxide Layer:

Extends lifespan in high-temperature applications.


● Eco-Certified:

Compliant with RoHS, REACH, ISO 9001, and AS9100.



Typical Applications


● Chemical Equipment:

Acid bath heaters, corrosive gas reactor elements.


● Industrial Furnaces:

Sintering furnace ribbons, metal heat treatment wires.


● Aerospace:

Rocket nozzle heaters, high-temp test bench modules.


● New Energy:

Nuclear heating systems, energy storage thermal controls.



Technical Specifications


ParameterNumericUnit
Melting Point1370-1400℃
Tensile Strength≥780MPa
Elongation≥20%
Surface FinishBright Annealed / Pickled-
Thickness Range0.1-12.0mm
Width Range5-200mm



Target Industries


● Chemical & Petrochemical

● Industrial High-Temp Processing

● Aerospace & Defense

● New Energy & Nuclear



Packaging & Certifications


● Anti-Corrosion Packaging:

Vacuum aluminum foil bags with desiccants.


● Certifications:

ISO 9001, AS9100, RoHS, REACH, SGS reports.



Why Choose Us?


● Technical Excellence:

25+ years in NiCr alloy R&D and high-temp solutions.


● Fast Turnaround:

72-hour sample delivery, 10-18 days for custom orders.


● Global Reach:

Serving 80+ countries with localized logistics hubs.



Available Forms


We provide you with a variety of product forms, including but not limited to


● Strip & Foil

● Round Wire &Flat Wire

● Bar & Rod

● Electrothermal Strip

● Flange & Ring

● Wire & Welding

● Reststance Wire

● Electric Alloy Wire

● Electric Furnace Bar

● Customize

description2

Leave Your Message