Leave Your Message
Products Categories
Featured Module

Precision Alloys Wire 4J342(4J42)

  • Place of Origin Jiangsu,China
  • Model Number Precision Alloys Wire 4J342(4J42)
  • Trade Names Iron chromium aluminum electrothermal alloy wire
  • Dimensions Customized Size
  • Delivery Conditions Grinding. Polished. Bright.
  • Avaliable Shapes Wire.Customized
  • MOQ 50~200 (KG)
  • Production Standards GB/T、GJB、YB/T、ASTM、EN、DIN、IEC
  • Packaging Details Wooden Case, or as per Client's request
  • Payment Terms L/C, T/T, Western Union, MoneyGram
  • Trade Terms FOB, CIF, DDP, DAP, EXW
  • Delivery Time 20~60 days

Overview

Precision Alloys Wire 4J342(4J42) is a kind of fe-chromium-aluminum electric heating alloy round wire.



Limiting Chemical Composition, %


Chromium..................................................................................................................................12.0-15.0

Aluminum.................................................................................................................................4.0-6.0

The rest is iron



Main Properties


Alloy Nomenclature → 0Cr27Al7Mo2 0Cr21Al6Nb FCHW-1
0Cr25Al5
0Cr23Al5
0Cr21Al6 FCHW-2
0Cr21Al4
0Cr19Al3
1Cr13Al4
Performance ↓
Main chemical composition Cr 26.5-27.8 21-23 23.5-26 19-22 17-21 12-15
Al 6-7 5-7 4.5-6.5 5-7 3-4.2 4-6
Fe Rest Rest Rest Rest Rest Rest
Else Mo quantity added to :1.8-2.2 Nb quantity added to : 0.5 —— —— —— ——
Max.Continuous service
temp.of element(℃)
1400 1350 1250 1250 1100 950
(Ω·mm²/m)
Resistivity at20℃
1.53 1.45 1.42 1.42 1.23 1.25
Density(g/cm³) 7.1 7.1 7.1 7.16 7.35 7.4



Physical Constants


Density

about 7.4g/cm³

Thermal conductivity

52.7kJ/m·h·℃

15.4×10⁻⁶/℃

Linear expansion coefficient



Performance feature


● High resistivity:

at 20℃, the resistivity is about 1.25±0.08μΩ · m, and larger alloy materials can be used in the design of heating elements, which is conducive to extending the service life of components.


● Low resistance temperature coefficient:

The resistance changes relatively little with the temperature, and can maintain relatively stable resistance performance under different temperature environments, so as to ensure that the heating power of the heating element is relatively stable.


● High temperature resistance:

The maximum operating temperature can reach 950℃, with good high temperature stability.


● Good oxidation resistance:

Under high temperature, a dense Al₂O₃ oxide film can be formed on its surface, which has a dense structure, good adhesion to the matrix, and is not easy to fall off, and has excellent oxidation resistance to effectively prevent further oxidation corrosion of the alloy.


● Good sulfur resistance:

good corrosion resistance to sulfur-containing atmosphere and surface contaminated by sulfur-containing substances.


Application field


● Brake resistance:

mainly used in electric locomotives, diesel locomotives, subway vehicles and high-speed train braking system brake resistance.


● Heating elements:

such as heating elements for kitchen appliances such as ceramic stoves, and heating wires in high temperature heating equipment such as industrial furnaces.



Available Forms


We provide you with a variety of product forms, including but not limited to


● Strip & Foil

● Round Wire &Flat Wire

● Bar & Rod

● Electrothermal Strip

● Flange & Ring

● Wire & Welding

● Reststance Wire

● Electric Alloy Wire

● Electric Furnace Bar

● Customize

description2

Leave Your Message