Nickel-chromium Alloys Wire Cr15Ni60

  • Place of Origin Jiangsu,China
  • Model Number Nickel-chromium Alloys Wire Cr15Ni60
  • Trade Names Cr15Ni60,Ni60Cr15
  • Dimensions Customized Size
  • Delivery Conditions Grinding. Polished. Bright.
  • Avaliable Shapes Wire.Customized
  • MOQ 50~200 (KG)
  • Production Standards GB/T、GJB、YB/T、ASTM、EN、DIN、IEC
  • Packaging Details Wooden Case, or as per Client's request
  • Payment Terms L/C, T/T, Western Union, MoneyGram
  • Trade Terms FOB, CIF, DDP, DAP, EXW
  • Delivery Time 20~60 days

Overview

Cr15Ni60 nickel chromium alloy round wire is a cost-effective solution for electric heating elements and appliances. With high resistivity and excellent thermal properties, it is widely used in household heating devices and industrial heating systems.



Limiting Chemical Composition, %


Chromium(Cr)..................................................................................................................................15.0

Nickel(Ni).........................................................................................................................................60.0

Balance Iron (Fe) & Trace Elements



Main Properties


Alloy Nomenclature → Cr20Ni80 Cr30Ni70 Cr15Ni60 Cr20Ni35 Cr20Ni30 Cr25Ni20
Performance ↓
Main chemical composition Ni Rest Rest 55-61 34-37 30-34 19-22
Cr 20-23 28-31 15-18 18-21 18-21 23-27
Fe ≤1.0 ≤1.0 Rest Rest Rest Rest
Max.Continuous service
temp.of element(℃)
1200 1250 1150 1100 1100 950
(Ω·mm²/m)
Resistivity at20℃
1.09 1.18 1.12 1.04 1.04 0.96
Density(g/cm³) 8.4 8.1 8.2 7.9 7.9 8



Material Characteristics


Density

about 8.2g/cm³

Resistivity

1.32 μΩ·m (20℃)

Temperature Range

Continuous Service 800℃~1000℃, Short-Term Peak 1100℃



Key Advantages


● Energy-Efficient Heating:

Ultra-high resistivity enables rapid heating, reducing energy consumption by 20% compared to conventional heating alloys.


● Corrosion Resistance:

60% nickel improves resistance to sulfurization and chloride attack, suitable for humid and chemical environments.


● Processing Flexibility:

Superior ductility (≥30% elongation) supports complex coil winding and precision heating component fabrication.


Typical Applications


● Household Heating Components:

Spiral heating wires and heating discs for electric kettles, microwaves, and irons.


● Industrial Temperature Control:

Heating bands for plastic injection molding machines, temperature modules for packaging equipment, laboratory drying ovens.


● Electronics & New Energy:

Heating wires for lithium battery drying furnaces, preheating elements in semiconductor equipment.



Material Characteristics


ParameterNumericUnit
Melting Point1350-1380℃
Tensile Strength≥580MPa
Elongation≥30%
Surface FinishBright/Matte-
Diameter Range0.1-4.0mm



Target Industries


● Household Appliances & Consumer Electronics

● Plastics Processing & Packaging

● New Energy & Semiconductor

● Laboratory Equipment



Packaging & Certifications


● Packaging:

Anti-static spools/custom-cut packaging, ≤200m/coil (small sample orders available).


● Certifications:

IEC 60539, RoHS, UL Certification (compliant with appliance safety standards).



Why Choose Cr15Ni16?


● Household Appliance Benchmark:

Tailored for compact, energy-efficient appliances, meeting UL/IEC safety standards to accelerate product launch.


● Cost Leadership:

Outstanding price-performance ratio among high-nickel alloys, compatible with automated mass production.



Available Forms


We provide you with a variety of product forms, including but not limited to


● Strip & Foil

● Round Wire &Flat Wire

● Bar & Rod

● Electrothermal Strip

● Flange & Ring

● Wire & Welding

● Reststance Wire

● Electric Alloy Wire

● Electric Furnace Bar

● Customize

description2

Leave Your Message