- Fe-Cr-Al Alloys
- Nickel-chromium Alloys
- Cn/Mn-Cu Alloys
- Cu-Ni Alloys
- Precision Alloys
- Ni-Al Alloys
- Pure Nickel Alloys
- Monel Alloys
- Hastelloy Alloys
- Inconel Alloys
- Incoloy Alloys
- Haynes Alloys
Fe-Cr-Al Alloys Flat Wire 0Cr21Al6Nb
Overview
Fe-Cr-Al Alloys Flat Wire 0Cr21Al6Nb is a kind of electrothermal alloy material with specific chemical composition, physical properties and applications.
Limiting Chemical Composition, %
Chromium..................................................................................................................................12.0-15.0
Aluminum.................................................................................................................................4.0-6.0
The rest is iron
Main Properties
| Alloy Nomenclature → | 0Cr27Al7Mo2 | 0Cr21Al6Nb | FCHW-1 0Cr25Al5 0Cr23Al5 |
0Cr21Al6 | FCHW-2 0Cr21Al4 0Cr19Al3 |
1Cr13Al4 | |
| Performance ↓ | |||||||
| Main chemical composition | Cr | 26.5-27.8 | 21-23 | 23.5-26 | 19-22 | 17-21 | 12-15 |
| Al | 6-7 | 5-7 | 4.5-6.5 | 5-7 | 3-4.2 | 4-6 | |
| Fe | Rest | Rest | Rest | Rest | Rest | Rest | |
| Else | Mo quantity added to :1.8-2.2 | Nb quantity added to : 0.5 | —— | —— | —— | —— | |
| Max.Continuous service temp.of element(℃) |
1400 | 1350 | 1250 | 1250 | 1100 | 950 | |
| (Ω·mm²/m) Resistivity at20℃ |
1.53 | 1.45 | 1.42 | 1.42 | 1.23 | 1.25 | |
| Density(g/cm³) | 7.1 | 7.1 | 7.1 | 7.16 | 7.35 | 7.4 | |
Physical Properties
The alloy has high plasticity at room temperature, good cold stamping performance, but the welding performance is not good. The alloy is a ferrite structure after annealing treatment, the structure is unstable during use, 475℃ is its brittle temperature zone, long-term heating will lead to coarse grains.
Resistance and temperature characteristics
0Cr21Al6Nb alloy has high resistivity and moderate temperature coefficient. It can maintain good oxidation resistance and thermal strength below 800 ° C.
Application
Due to the properties of 0Cr21Al6Nb alloy, it is mainly used as a heating element in heat treatment furnaces below 750 ° C. In addition, it can also be used for low-grade electric heat pipes and low-grade household electric heaters, as well as resistance bands in resistance boxes.
Announcement
When in use, long-term overtemperature and overload should be avoided to prevent the performance of the alloy from decreasing or damaging. At the same time, when operating at high temperatures, it is necessary to pay attention to safety and avoid direct contact with the high-temperature alloy belt to prevent burns or other safety accidents.
Available Forms
We provide you with a variety of product forms, including but not limited to
● Strip & Foil
● Round Wire &Flat Wire
● Bar & Rod
● Electrothermal Strip
● Flange & Ring
● Wire & Welding
● Reststance Wire
● Electric Alloy Wire
● Electric Furnace Bar
● Customize
description2

1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
6J12
6J8
6J13
6J40
CuMn7SN
CuMn30Ni5
6J12
6J8
6J13
6J40
CuMn7SN
CuMn30Ni5
6J12
6J8
6J13
6J40
CuMn7SN
CuMn30Ni5
6J12
6J8
6J13
6J40
CuMn7SN
CuMn30Ni5
CuNi30
CuNi34
CuNi44
CuNi30
CuNi34
CuNi44
CuNi30
CuNi34
CuNi44
CuNi30
CuNi34
CuNi44
4J336(4J36)
4J342(4J42)
4J343(4J43)
4J352(4J49)
4J350(4J50)
6J415(6J15)
6J420(6J20)
6J422(6J22)
6J423(6J23)
6J424(6J24)
6J425(6J25)
6J426(6J26)
6J520(6J27)
4J336(4J36)
4J342(4J42)
4J343(4J43)
4J352(4J49)
4J350(4J50)
6J415(6J15)
6J420(6J20)
6J422(6J22)
6J423(6J23)
6J424(6J24)
6J425(6J25)
6J426(6J26)
6J520(6J27)
4J336(4J36)
4J342(4J42)
4J343(4J43)
4J352(4J49)
4J350(4J50)
6J415(6J15)
6J420(6J20)
6J422(6J22)
6J423(6J23)
6J424(6J24)
6J425(6J25)
6J426(6J26)
6J520(6J27)
6J525(6J28)
4J336(4J36)
4J342(4J42)
4J343(4J43)
4J352(4J49)
4J350(4J50)
6J415(6J15)
6J420(6J20)
6J422(6J22)
6J423(6J23)
6J424(6J24)
6J425(6J25)
6J426(6J26)
6J520(6J27)
6J525(6J28)
Ni95Al5
monel 400
monel R405
monel K500
monel 502
monel 400
monel R405
monel K500
monel 502
monel R405
monel K500
monel 502
Hastelloy C-22
Hastelloy C-22
Hastelloy C-22
Inconel 800
Inconel 800H
Inconel 800HT
Inconel 825
Inconel 800
Inconel 800H
Inconel 800HT
Inconel 825
Inconel 800
Inconel 800H
Inconel 800HT
Inconel 825
Strip & Foil
Round Wire
Bar & Rod
Electrothermal strip
Bolts & Fasteners
Flange & Ring
Wire & Welding
Reststance wire & flat wire
Electric alloy wire
Electric furnace wire