F1 Manganin Constantan copper Alloys Bar 6J8

  • Place of Origin Jiangsu,China
  • Model Number F1 Manganin Constantan copper Alloys Bar 6J8
  • Trade Names UNS C96400 Bar, 2.1290 Bar
  • Dimensions Customized Size
  • Delivery Conditions Grinding. Polished. Bright.
  • Avaliable Shapes Bar.Rod.Customized
  • MOQ 50~200 (KG)
  • Production Standards GB/T、GJB、YB/T、ASTM、EN、DIN、IEC
  • Packaging Details Wooden Case, or as per Client's request
  • Payment Terms L/C, T/T, Western Union, MoneyGram
  • Trade Terms FOB, CIF, DDP, DAP, EXW
  • Delivery Time 20~60 days

Overview

F1 Manganin Constantan copper Alloys Bar 6J8 is engineered for harsh industrial environments, combining enhanced manganese-copper (Mn-Cu) ratios for superior mechanical strength, corrosion resistance, and stable conductivity. With optimized resistivity (0.02-0.03 Ω·mm²/m) and heat tolerance (continuous use at 350°C), it is ideal for precision electronics, high-temperature sensors, and chemical processing equipment. ISO 9001 certified, 6J8 wire guarantees long-term reliability and eco-compliance.



Limiting Chemical Composition, %


Nickel(Ni)................................................................................................................................................—

Manganese(Mn).............................................................................................................................8.0-10.0

Copper(Cu)............................................................................................................................................Rest

The Else is Si including 1.0-2.0.



Main Properties


Performance / Nomenclature Constantan 6J40 Novokonstant 6J11 Manganin 6J12  F1 Manganin 6J8          F2 Manganin 6J13        
Main chemical composition Ni 39.0-41.0 — 2.0-3.0 — 2.0-5.0
Mn 1.0-2.0 10.5-12.5 11.0-13.0 8.0-10.0 11.0-13.0
Cu Rest Rest Rest Rest Rest
Else — Al:2.5-4.5
Fe:1.0-1.6
— Si:1.0-2.0 —
Service temperature
(℃)
5-500 5-500 5-450 10-480 10-480
Density
(g/cm³)
8.88 8 8.44 8.7 8.4
Resistivity at20℃
(200Cμ.m)
0.48±0.03 0.48±0.03 0.46±0.03 0.35±0.05 0.44±0.04
Temperature coefficient
x10-6/℃(20-600℃)
+40 +80 +20 +10 40
-40 -80 -3 -5
P-copper thermoelectric potential
(μV/℃)(0-100℃)
45 2 1 2 2
Elongation at rupture(%) ≥15 ≥15 ≥15 ≥15 ≥15



Technical Specifications


Parameter

Value/Range

Melting Point

980-1080°C

Tensile Strength

600-750 MPa

Elongation

15-22%

Surface Finish

Mirror Polish/Passivated

Diameter Range

Customized (10.0mm-300.0mm)

Temperature Resistance

-60°C ~ 350°C

Continuous Use Temp

≤350°C

Short-Term Peak Temp

≤500°C (≤15 mins)

Resistivity

0.025-0.030 Ω·mm²/m

Density

8.4-8.8 g/cm³



Material Properties


● High Strength & Fatigue Resistance:

Tensile strength 600-750 MPa for dynamic loads.


● Corrosion & Oxidation Resistance:

Resists chemical erosion and high-temperature oxidation.


● Stable Conductivity:

Minimal resistivity variation for precise signal transmission.


● Broad Temperature Range:

Operates from -60°C to 350°C.


Core Advantages


● Industrial Durability:

Performs in high-vibration, humid, and chemical environments.


● Precision Fabrication:

Compatible with micron-level wire drawing and forming.


● Rapid Delivery:

Custom small batches and global 48-hour samples.



Typical Applications


● Electronics Packaging:

IC lead frames, micro-connectors.


● Energy Systems:

Fuel cell bipolar plates, high-temperature electrodes.


● Chemical Processing:

Corrosion-resistant reactor linings, pump valves.


● Automotive EV:

Battery connectors, sensor wiring.



Industries Served


● Consumer Electronics & Semiconductor Packaging

● New Energy & Hydrogen Systems

● Chemical & Marine Engineering

● Automotive & Rail Transport

● Medical Implant Devices



Packaging & Certifications


● ESD-Safe Packaging: Vacuum-sealed spools with desiccants for cleanrooms.

● Certifications: ISO 9001, RoHS, REACH, ASTM B105 compliant.



Why Choose 6J8?


● Harsh Environment Certified:

Passed 1000hr salt spray and thermal cycling tests.


● Global Supply Chain:

Regional warehouses in EU/US/Asia for fast logistics.


● Co-Development Support:

Material selection and failure analysis services.



Available Forms


We provide you with a variety of product forms, including but not limited to


● Strip & Foil

● Round Wire &Flat Wire

● Bar & Rod

● Electrothermal Strip

● Flange & Ring

● Wire & Welding

● Reststance Wire

● Electric Alloy Wire

● Electric Furnace Bar

● Customize

description2

Leave Your Message