Nickel-chromium Alloys Electrothermal strip Cr25Ni20

  • Place of Origin Jiangsu,China
  • Model Number Nickel-chromium Alloys Electrothermal strip Cr25Ni20
  • Trade Names High Nickel-Chromium Alloy Electrothermal Strip
  • Dimensions Customized Size
  • Delivery Conditions Grinding. Polished. Bright.
  • Avaliable Shapes Wire.Customized
  • MOQ 50~200 (KG)
  • Production Standards GB/T、GJB、YB/T、ASTM、EN、DIN、IEC
  • Packaging Details Wooden Case, or as per Client's request
  • Payment Terms L/C, T/T, Western Union, MoneyGram
  • Trade Terms FOB, CIF, DDP, DAP, EXW
  • Delivery Time 20~60 days

Overview

The Cr25Ni20 Nickel-Chromium Electrothermal Strip is designed for extreme high-temperature environments, with 25% chromium and 20% nickel. It offers excellent oxidation resistance and high resistivity, ideal for industrial furnaces, heat treatment equipment, and glass manufacturing, with a sustained operating temperature up to 1200°C.



Limiting Chemical Composition, %


Chromium(Cr)..................................................................................................................................25.0

Aluminum(Ni)..................................................................................................................................20.0

Balance Iron (Fe) & Trace Elements



Main Properties


Alloy Nomenclature → Cr20Ni80 Cr30Ni70 Cr15Ni60 Cr20Ni35 Cr20Ni30 Cr25Ni20
Performance ↓
Main chemical composition Ni Rest Rest 55-61 34-37 30-34 19-22
Cr 20-23 28-31 15-18 18-21 18-21 23-27
Fe ≤1.0 ≤1.0 Rest Rest Rest Rest
Max.Continuous service
temp.of element(℃)
1200 1250 1150 1100 1100 950
(Ω·mm²/m)
Resistivity at20℃
1.09 1.18 1.12 1.04 1.04 0.96
Density(g/cm³) 8.4 8.1 8.2 7.9 7.9 8



Material Characteristics


Density

about 8.4g/cm³

Resistivity

1.28 μΩ·m (20℃)

Temperature Range

Continuous Service 1150℃~1300℃, Short-Term Peak 1350℃



Key Advantages


● Dual High-Content Reinforcement:

30% Cr + 70% Ni synergy provides triple protection against carburization, sulfidation, and extreme-temperature oxidation.


● Extreme Mechanical Strength:

Maintains ≥200 MPa tensile strength at 1300℃, resisting high-temperature creep deformation.


● Superior Chemical Inertness:

Corrosion rate <0.1 mm/year in strong acids, alkalis, and halogen-containing atmospheres.


Typical Applications


● Chemical Reactors:

Heating elements and catalyst carrier wires for ethylene cracking furnaces and ammonia synthesis reactors.


● Nuclear Energy Systems:

Heating wires for reactor control rods, resistance components in high-temperature cooling circuits.


● Special Metallurgy:

Radiant tubes and heating coils for tungsten-molybdenum sintering furnaces and superalloy melting systems.



Technical Specifications


ParameterNumericUnit
Melting Point1450-1480℃
Tensile Strength≥750MPa
Elongation≥15%
Surface FinishBright/Electropolished-
Diameter Range0.3-10.0mm



Target Industries


● Chemical & Petrochemical

● Nuclear & New Energy

● Special Metallurgy & Aerospace

● Semiconductor Fabrication



Packaging & Certifications


● Packaging:

Double-layer vacuum moisture-proof packaging/stainless steel spools, ≤100m/coil (ultra-clean processing available).


● Certifications:

ASME SB166, ISO 6208, NACE MR0175, Compliant with ASME III for Nuclear Applications.



Why Choose Cr25Ni20?


● Strategic Material Alternative:

Replaces Inconel 600 in carburizing/sulfidizing environments with 30% cost reduction.


● Full Lifecycle Support:

High-temperature performance simulation, failure analysis, and custom pre-oxidized coatings (Al₂O₃/SiO₂).



Available Forms


We provide you with a variety of product forms, including but not limited to


● Strip & Foil

● Round Wire &Flat Wire

● Bar & Rod

● Electrothermal Strip

● Flange & Ring

● Wire & Welding

● Reststance Wire

● Electric Alloy Wire

● Electric Furnace Bar