The smelting process of nickel alloys
2024-10-02
The melting process of nickel alloys is a complex and delicate operation, which usually includes the following key steps:
- Melting methods: Nickel-based alloys are usually melted using methods such as Vacuum Induction Melting (VIM), Electroslag Remelting (ESR) and Vacuum Autoclave Arc Melting (VAR). These methods can maintain the purity of the alloy at high temperatures while preventing oxidation and contamination of the alloy components.
- Preparation before melting: Before melting, raw materials need to be pre-treated, such as drying to remove moisture and impurities to minimize porosity and inclusions during the melting process.
- Melting process control: During the melting process, the melting temperature and atmosphere need to be precisely controlled to ensure the chemical composition and physical properties of the alloy. Inert gas protection, such as argon, is usually used to prevent the alloy from coming into contact with air, thus avoiding oxidation.
- Post-melting processing: After melting is complete, the alloy is usually subjected to forging, rolling, or other thermal processes to improve its microstructure and mechanical properties. These processes can break the casting organization, optimize the microstructure.
- Heat treatment: Nickel-based alloys usually require heat treatment after processing, including solid solution treatment and aging treatment, to obtain the desired mechanical properties and corrosion resistance. Solid solution treatment can dissolve back precipitated phases to improve toughness and resistance to sublimation, while aging treatment can precipitate reinforcing phases to improve strength.
- Quality control: Stringent quality control throughout the melting process, including chemical composition analysis, metallurgical organization checking and property testing, is required to ensure that the alloy meets the requirements of the specific application.
Nickel-based alloys are widely used in aerospace, chemical and energy industries due to their excellent strength and corrosion resistance at high temperatures. Optimization of the melting process is critical to improving alloy properties.

1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
1Cr13Al4
0Cr15Al5
0Cr19Al2
0Cr21Al4
0Cr21Al6
0Cr25Al5
0Cr21Al6Nb
0Cr27Al7Mo2
6J12
6J8
6J13
6J40
CuMn7SN
CuMn30Ni5
6J12
6J8
6J13
6J40
CuMn7SN
CuMn30Ni5
6J12
6J8
6J13
6J40
CuMn7SN
CuMn30Ni5
6J12
6J8
6J13
6J40
CuMn7SN
CuMn30Ni5
CuNi30
CuNi34
CuNi44
CuNi30
CuNi34
CuNi44
CuNi30
CuNi34
CuNi44
CuNi30
CuNi34
CuNi44
4J336(4J36)
4J342(4J42)
4J343(4J43)
4J352(4J49)
4J350(4J50)
6J415(6J15)
6J420(6J20)
6J422(6J22)
6J423(6J23)
6J424(6J24)
6J425(6J25)
6J426(6J26)
6J520(6J27)
4J336(4J36)
4J342(4J42)
4J343(4J43)
4J352(4J49)
4J350(4J50)
6J415(6J15)
6J420(6J20)
6J422(6J22)
6J423(6J23)
6J424(6J24)
6J425(6J25)
6J426(6J26)
6J520(6J27)
4J336(4J36)
4J342(4J42)
4J343(4J43)
4J352(4J49)
4J350(4J50)
6J415(6J15)
6J420(6J20)
6J422(6J22)
6J423(6J23)
6J424(6J24)
6J425(6J25)
6J426(6J26)
6J520(6J27)
6J525(6J28)
4J336(4J36)
4J342(4J42)
4J343(4J43)
4J352(4J49)
4J350(4J50)
6J415(6J15)
6J420(6J20)
6J422(6J22)
6J423(6J23)
6J424(6J24)
6J425(6J25)
6J426(6J26)
6J520(6J27)
6J525(6J28)
Ni95Al5
monel 400
monel R405
monel K500
monel 502
monel 400
monel R405
monel K500
monel 502
monel R405
monel K500
monel 502
Hastelloy C-22
Hastelloy C-22
Hastelloy C-22
Inconel 800
Inconel 800H
Inconel 800HT
Inconel 825
Inconel 800
Inconel 800H
Inconel 800HT
Inconel 825
Inconel 800
Inconel 800H
Inconel 800HT
Inconel 825
Strip & Foil
Round Wire
Bar & Rod
Electrothermal strip
Bolts & Fasteners
Flange & Ring
Wire & Welding
Reststance wire & flat wire
Electric alloy wire
Electric furnace wire